Polymer Property : Viscosity = 92900 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 92900 cP

@Shear Rate 5000 1/s,
Temperature 250 °C
92900 cP

@Shear Rate 5000 1/s,
Temperature 482 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET  (Unverified Data**)
82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers