Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 94140 cP @Shear Rate 5000 1/s, Temperature 290 °C |
94140 cP @Shear Rate 5000 1/s, Temperature 554 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers |