Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 950000 cP @Shear Rate 1000 1/s, Temperature 240 °C |
950000 cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
DSM Akulon® F230-C PA6 Medium Viscosity, Extrusion, Injection Molding |