Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 98500 cP @Shear Rate 5000 1/s, Temperature 250 °C |
98500 cP @Shear Rate 5000 1/s, Temperature 482 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for Blow Molding Zytel LC6210 BK010 is a highly toughened heat stabilized polyamide 612 for extrusion blow molding or processing by other techniques requiring high .. |