Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00060 cm/cm | 0.00060 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® DP BKV 60 EF 000000 Nylon6, 60% Glass Fiber PA 6, 60% glass fibers, injection molding, improved flowabilityInformation provided by LANXESS. |