Polymer Property : Linear Mold Shrinkage, Transverse = 0.0014 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0014 cm/cm
0.0014 in/in
ISO 294-4, 2577
Lanxess Durethan® DP 1802 H3.0 000000 Nylon 6
PA 6 injection and extrusion molding grade, non-reinforced, impact-modified, UL 94V-2 off 0,75 mm, GWIT: 775°C off 0,75 mm, halogen-free
Linear Mold Shrinkage, Transverse 0.0014 cm/cm
0.0014 in/in
ISO 294-4, 2577
Lanxess Durethan® DP BC 500 H2.0 901510 Nylon 6
PA 6, extrusion and blow molding grade, non-reinforced, elastomer-modified, high viscosity, good heat-ageing resistance
Linear Mold Shrinkage, Transverse 0.0014 cm/cm
0.0014 in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
Lanxess Durethan® BKV 30 H2.0 EF DUS029 901510 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.
Linear Mold Shrinkage, Transverse 0.0014 cm/cm
0.0014 in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
Lanxess Durethan® DP BKV 35 XF 901510 Nylon 6, 35% Glass Fiber
PA 6, 35% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS.
Linear Mold Shrinkage, Transverse 0.0014 cm/cm
0.0014 in/in
ISO 294-4
Solvay Specialty Polymers Kalix® 3950 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 3950 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in..