Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0019 cm/cm
0.0019 in/in
STN EN ISO 294-4
Plastcom PLASTAMID® 66 GF 20 PA66 reinforced with glass fiber
PA66 reinforced with 20 % glass fiber, used in the automotive, engineering and electrical industry. Application: hobby tools, covers of electrotools, electromotors, cooling screws of blowers, gear w..
Linear Mold Shrinkage, Transverse 0.0019 cm/cm
0.0019 in/in
STN 64 0808
Plastcom SLOVAMID 66 CF 20 Polyamide 66, 20% Carbon Fiber
FeaturesChemically reinforced with 20% carbon fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. ..
Linear Mold Shrinkage, Transverse 0.0019 cm/cm
0.0019 in/in
Plastcom SLOVAMID 66 GF 20 PA66, 20% glass fibre
FeaturesChemically reinforced with 20 % glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. ..
Linear Mold Shrinkage, Transverse 0.0019 cm/cm
0.0019 in/in
Plastcom SLOVAMID 66/6 GF 20 PA66/6, 20% glass fibre
FeaturesChemically reinforced alloy PA 66 and PA 6 with 20 % glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and ..
Linear Mold Shrinkage, Transverse 0.0019 cm/cm
0.0019 in/in
ISO 294-4, 2577
Lanxess Pocan® S 7926 000000 PBT
PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified
Linear Mold Shrinkage, Transverse 0.0019 cm/cm
0.0019 in/in
GB/T 15585-1995
Sichuan Deyang Haton® hCF41 Polyphenylene Sulfide
Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD
Linear Mold Shrinkage, Transverse 0.0019 cm/cm

@Thickness 3.20 mm
0.0019 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Transverse 0.0019 cm/cm

@Thickness 3.20 mm
0.0019 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR