Polymer Property : Linear Mold Shrinkage, Transverse = 0.0023 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0023 cm/cm
0.0023 in/in
ISO 294-4, 2577
Lanxess Pocan® DP 2004 000000 PBT
PBT, non-reinforced, injection molding, halogen free flame retardant