Polymer Property : Linear Mold Shrinkage, Transverse = 0.0034 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0034 - 0.0054 cm/cm

@Time 86400 sec
0.0034 - 0.0054 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Verton NV0041EV_GY7E147 PC+ABS
Preliminary data for 20% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.0034 - 0.0054 cm/cm

@Time 86400 sec
0.0034 - 0.0054 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS
Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.