Polymer Property : Linear Mold Shrinkage, Transverse = 0.0036 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0036 cm/cm
0.0036 in/in
Plastcom SLOVAMID 6/66 GF 20 T 10 FRG 5 PA6/66, 20% glass fibre, flame retardant
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Linear Mold Shrinkage, Transverse 0.0036 cm/cm
0.0036 in/in
ISO 294-4
Solvay TECHNYL® A 218G V33 Black 34N PA66, 25% glass fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail..
Linear Mold Shrinkage, Transverse 0.0036 - 0.0042 cm/cm

@Time 86400 sec
0.0036 - 0.0042 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon EX08308C PEI (Asia Pacific)
Stat-Kon* EX08308C is a high cleanliness Polyetherimide Compound reinforced with Carbon Fiber for use in applications requiring the highest level of cleanliness. This compound is compounded using LN..
Linear Mold Shrinkage, Transverse 0.0036 cm/cm
0.0036 in/in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON EX07311P PEI (Asia Pacific)
LNP Stat-kon* EX07311P is an easy flowing ESD-safe compound based on Polyetherimide resin. This compound is developed for good dimensional stability for use in ESD Tray for Backend Semicon and HDD t..
Linear Mold Shrinkage, Transverse 0.0036 cm/cm

@Time 86400 sec
0.0036 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DC0041PQ PC
LNP* THERMOCOMP* DC0041PQ is a compound based on Polycarbonate resin containing Carbon Fiber. Added feature of this grade is: Flame Retardant.