Polymer Property : Linear Mold Shrinkage, Transverse = 0.0037 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0037 cm/cm
0.0037 in/in
ISO 294-4
DuPont Performance Polymers Hytrel® 4053FG TPC-ET  (Unverified Data**)
Hytrel® 4053FG is a low modulus high performance thermoplastic elastomer with food compliance specificity. It is suitable for extrusion and injection molding processes.Information provided by DuPon..