Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00550 - 0.0100 cm/cm
0.00550 - 0.0100 in/in
Average value: 0.00700 cm/cm Grade Count:5
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..