Polymer Property : Linear Mold Shrinkage, Transverse = 0.00590 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00590 - 0.0140 cm/cm
0.00590 - 0.0140 in/in
Average value: 0.00989 cm/cm Grade Count:11
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..