Linear Mold Shrinkage, Transverse 0.0069 cm/cm
0.0069 in/in
Plastcom SLOVAMID 6 NG GF 20 HLS PA6, 20% glass fibre, combined stability
FeaturesPA 6 for injection moulding, chemically reinforced with 20% glass fibre, heat stabilized and weather stabilized. Stabilized against hydrolysis. Good surface finisch.Packaging, transport, sto..
Linear Mold Shrinkage, Transverse 0.0069 cm/cm

@Temperature 80.0 °C
0.0069 in/in

@Temperature 176 °F
60x60x2 mm; ISO 294-4
Gromax BFG30-FU00B3 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Linear Mold Shrinkage, Transverse 0.0069 cm/cm
0.0069 in/in
ISO 294-4, 2577
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures