Polymer Property : Linear Mold Shrinkage, Transverse = 0.0078 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0078 cm/cm
0.0078 in/in
Plastcom SLOVAMID 6 GF 25 FRG 5 PA6, 25% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°..
Linear Mold Shrinkage, Transverse 0.0078 cm/cm
0.0078 in/in
STN 64 0808
Plastcom SLOVAMID 6 GF 10 FRG 5 Polyamide 6, 10% Glass Fiber, Flame Retardant
FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fiber. Application: impacted mouldings with high strength applied in automotive, electrical, engineering and consumer-goo..
Linear Mold Shrinkage, Transverse 0.0078 cm/cm
0.0078 in/in
Plastcom SLOVAMID 6 NG GF 15 HI PA6, 15% glass fibre, improved strength
FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..
Linear Mold Shrinkage, Transverse 0.0078 cm/cm
0.0078 in/in
GB/T 15585-1995
Sichuan Deyang Haton® hGR302 PPS / F4 Polyphenylene Sulfide
Injection molding, anti-frictionInformation provided by Sichuan Deyang Chemical Co., LTD
Linear Mold Shrinkage, Transverse 0.0078 cm/cm
0.0078 in/in
GB/T 15585-1995
Sichuan Deyang Haton® hGR31M1 Polyphenylene Sulfide
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD
Linear Mold Shrinkage, Transverse 0.0078 cm/cm

@Thickness 3.20 mm
0.0078 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Starex® WX-9700 ASA, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Transverse 0.0078 cm/cm

@Thickness 3.20 mm
0.0078 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Starex® WX-9700 ASA, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.