Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0081 cm/cm
0.0081 in/in
Plastcom SLOVAMID 6 GF 20 FRG 3 PA6, 20% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 20 % glass fibre, with halogen free flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 9..
Linear Mold Shrinkage, Transverse 0.0081 cm/cm
0.0081 in/in
60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance
Linear Mold Shrinkage, Transverse 0.0081 cm/cm
0.0081 in/in
150x105x3; 280°C / MT 80°C; 500 bar; ISO 2577
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Linear Mold Shrinkage, Transverse 0.0081 - 0.0083 cm/cm

@Time 86400 sec
0.0081 - 0.0083 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6
LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity.
Linear Mold Shrinkage, Transverse 0.0081 - 0.0083 cm/cm

@Time 86400 sec
0.0081 - 0.0083 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6
4.0 specific gravity, Nylon 6
Linear Mold Shrinkage, Transverse 0.0081 cm/cm

@Time 86400 sec
0.0081 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON MV005SX0 PP (Europe-Africa-Middle East)
LNP* VERTON* MV005SX0 is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized.