Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00300 - 0.00850 cm/cm | 0.00300 - 0.00850 in/in | Average value: 0.00512 cm/cm Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Linear Mold Shrinkage, Transverse | 0.00520 - 0.00850 cm/cm | 0.00520 - 0.00850 in/in | Average value: 0.00657 cm/cm Grade Count:3 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |