Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0091 cm/cm
0.0091 in/in
Plastcom SLOVAMID 66 GF 13 TS PA66, 13% glass fibre
FeaturesChemically reinforced with 13% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W..
Linear Mold Shrinkage, Transverse 0.0091 cm/cm
0.0091 in/in
ISO 294-4, 2577
Lanxess Durethan® AKV 35 H2.0 901510 Nylon 66, 35% Glass Fiber
PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: gearbox oil sumps, oil modules
Linear Mold Shrinkage, Transverse 0.0091 cm/cm
0.0091 in/in
ISO 294-4, 2577
Lanxess Pocan® DP BF 4232 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant
Linear Mold Shrinkage, Transverse 0.0091 - 0.0093 cm/cm

@Time 86400 sec
0.0091 - 0.0093 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Asia Pacific)
LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N..
Linear Mold Shrinkage, Transverse 0.0091 - 0.0093 cm/cm

@Time 86400 sec
0.0091 - 0.0093 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Europe-Africa-Middle East)
LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N..
Linear Mold Shrinkage, Transverse 0.0091 cm/cm
0.0091 in/in
60x60x2 mm; ISO 294
BASF Ultradur® S 4090 G4X 20% Glass Filled PBT