Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00500 - 0.00950 cm/cm
0.00500 - 0.00950 in/in
Average value: 0.00752 cm/cm Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..