Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0120 - 0.0215 cm/cm | 0.0120 - 0.0215 in/in | Average value: 0.0150 cm/cm Grade Count:7 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage, Transverse | 0.0120 cm/cm | 0.0120 in/in | Average value: 0.0120 cm/cm Grade Count:4 |
Overview of materials for Polymethylpentene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr.. |