Polymer Property : Linear Mold Shrinkage, Transverse = 0.0127 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0127 cm/cm
0.0127 in/in
STN EN ISO 294-4
Plastcom PLASTALEN® PH 91 T 20 Polypropylene reinforced with mineral filler
Modified homopolymer PP for injection molding with the content of 20 % mineral filler. General application in all industry branches. Delivered in natural mode and in the full RAL color scale.Informa..
Linear Mold Shrinkage, Transverse 0.0127 cm/cm
0.0127 in/in
Plastcom SLOVALEN PC 59 GF 30 PP, 30% glass fibre
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains themodifier of mechanical properties.Increased strength in comparison with unfilled PP. A..
Linear Mold Shrinkage, Transverse 0.0127 cm/cm
0.0127 in/in
Plastcom SLOVAMID 66 T 36 TS PA66, 36% mineral filling
FeaturesPA 66 with the content of 36 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel..
Linear Mold Shrinkage, Transverse 0.0127 cm/cm
0.0127 in/in
STN 64 0808
Plastcom SLOVASTER® B GF 20 Polybutylene Terephthalate, 20% Glass Fiber
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a..
Linear Mold Shrinkage, Transverse 0.0127 cm/cm
0.0127 in/in
Plastcom SLOVASTER® B1 GF 20 PBT, 20% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Linear Mold Shrinkage, Transverse 0.0127 cm/cm
0.0127 in/in
Plastcom SLOVASTER® B1 HML GF 20 PBT, 20% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Linear Mold Shrinkage, Transverse 0.0127 cm/cm
0.0127 in/in
STN EN ISO 294-4
Plastcom SLOVALEN PC 99 GF 30/1M Polypropylene reinforced with glass fiber, improved flowing
Modified copolymer PP for injection molding, reinforced with 30% glass fiber, improved flowing. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Informatio..
Linear Mold Shrinkage, Transverse 0.0127 cm/cm
0.0127 in/in
Plastcom SLOVASTER® B GB 20 M PBT, 20% glass beads
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..