Linear Mold Shrinkage, Transverse 0.000500 - 0.0141 cm/cm
0.000500 - 0.0141 in/in
Average value: 0.00707 cm/cm Grade Count:76
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Linear Mold Shrinkage, Transverse 0.0137 - 0.0141 cm/cm
0.0137 - 0.0141 in/in
Average value: 0.0139 cm/cm Grade Count:3
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..