Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0164 cm/cm | 0.0164 in/in | STN 64 0808 |
Plastcom SLOVAMID 66 GF 10 GB 20 Polyamide 66, 10% Glass Fiber, 20% Glass Beads FeaturesPA 66 chemically reinforced with 10% glass fiber and with the content of 20% glass beads. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical properties can .. |
|||
Linear Mold Shrinkage, Transverse | 0.0164 cm/cm @Thickness 2.00 mm |
0.0164 in/in @Thickness 0.0787 in |
TPE Method |
SCG Chemicals EL-Proâ„¢ P403J Polypropylene Injection Molding Key Characteristics:High stiffnessHigh glossGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfant articles, toys.. |
|||
Linear Mold Shrinkage, Transverse | 0.0164 cm/cm | 0.0164 in/in | ISO 2577 |
BASF Ultradur® B 4560 PBT Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF |