Polymer Property : Linear Mold Shrinkage, Transverse = 0.0186 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0186 cm/cm
0.0186 in/in
ISO 294-4
Solvay TECHNYL® C 236SI PA6, DRY
Description: Unreinforced polyamide 6 with high impact strength for injection molding.Available in: Europe and North AmericaProduct Applications: TECHNYL® C 236SI has high impact strength and fle..