Polymer Property : Linear Mold Shrinkage, Transverse = 0.0199 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0199 - 0.0239 cm/cm
0.0199 - 0.0239 in/in
ISO DIS 294-4
Wellman Wellamid® XT1573-N Impact Modified Nylon 66
Description: Impact Modified Nylon 66Information provided by Wellman.