Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0202 cm/cm
0.0202 in/in
Plastcom SLOVALEN PC 59 GB 10 PP, 10% glass beads
FeaturesCompouded homopolymer PP, with the content of 10% chemically bound glass beads and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry s..