Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0215 - 0.0235 cm/cm
0.0215 - 0.0235 in/in
LATI Latilub 73/13-10ST POM, Silicone/PTFE Filled
Self-lubricating product based on Polyoxymethylene (POM). Silicone / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri..