Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.000700 - 0.0590 cm/cm
0.000700 - 0.0590 in/in
Average value: 0.00787 cm/cm Grade Count:72
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..