Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.75 g/cc @Temperature 1450 °C, Time 7200 sec |
0.0994 lb/in³ @Temperature 2640 °F, Time 2.00 hour |
|
Chosun Refractories AU1 Blast Furnace Runner Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |