Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.80 g/cc @Temperature 200 °C |
0.101 lb/in³ @Temperature 392 °F |
|
Sharadaa Ceramics Sharada RFC-80 Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Bulk Density | 2.80 g/cc @Temperature 1400 °C |
0.101 lb/in³ @Temperature 2550 °F |
|
Sharadaa Ceramics Sharada RFC-95 Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Bulk Density | 2.80 g/cc @Temperature 800 °C |
0.101 lb/in³ @Temperature 1470 °F |
|
Sharadaa Ceramics Sharada RFC-90 Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Bulk Density | 2.80 g/cc @Temperature 110 °C, Time 86400 sec |
0.101 lb/in³ @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories AU1 Blast Furnace Runner Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.79 g/cc @Temperature 1000 °C, Time 10800 sec |
0.101 lb/in³ @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories M55 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.80 g/cc @Temperature 1500 °C, Time 10800 sec |
0.101 lb/in³ @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories RSP-M Blast Furnace Runner Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.79 g/cc @Temperature 110 °C, Time 86400 sec |
0.101 lb/in³ @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories SW88 Special High-Density Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |