Polymer Property : Bulk Density = 2.66 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 2.66 g/cc

@Temperature 1000 °C,
Time 10800 sec
0.0961 lb/in³

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories A65 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.66 g/cc

@Temperature 1500 °C,
Time 10800 sec
0.0961 lb/in³

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories A65 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.66 g/cc

@Temperature 1500 °C,
Time 10800 sec
0.0961 lb/in³

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories SR Blast Furnace Runner Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).