Polymer Property : Linear Mold Shrinkage = 0.0013 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0013 cm/cm

@Thickness 1.57 mm
0.0013 in/in

@Thickness 0.0618 in
Flow
DuPont Performance Polymers Rynite® FR543 NC010 PET
Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm..
Linear Mold Shrinkage 0.0013 cm/cm

@Thickness 1.57 mm
0.0013 in/in

@Thickness 0.0618 in
Flow; ASTM D955
DuPont Performance Polymers Rynite® 830ER NC010 PET
Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers