Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0017 cm/cm

@Thickness 1.57 mm
0.0017 in/in

@Thickness 0.0618 in
Flow
DuPont Performance Polymers Rynite® 940 BK505 PET  (Unverified Data**)
Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers