Polymer Property : Linear Mold Shrinkage = 0.012 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.010 - 0.012 cm/cm

@Thickness 3.17 mm
0.010 - 0.012 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.011 - 0.012 cm/cm

@Thickness 6.35 mm
0.011 - 0.012 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-60/TC/24/D/HS Polypropylene Homopolymer, Talc Filled, Heat Stabilized
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0060 - 0.012 cm/cm

@Thickness 1.00 mm
0.0060 - 0.012 in/in

@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0060 - 0.012 cm/cm

@Thickness 1.00 mm
0.0060 - 0.012 in/in

@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® T-662 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0060 - 0.012 cm/cm

@Thickness 1.00 mm
0.0060 - 0.012 in/in

@Thickness 0.0394 in
DAM
Toyobo T-661 Nylon 66, Standard Grade (Conditioned)
Features: Non-reinforced, Standard GradeInformation provided by Toyobo.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0090 - 0.012 cm/cm

@Thickness 1.00 mm
0.0090 - 0.012 in/in

@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® T-222SA Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0060 - 0.012 cm/cm

@Thickness 1.00 mm
0.0060 - 0.012 in/in

@Thickness 0.0394 in
Toyobo T-661 Nylon 66, Standard Grade (DAM)
Features: Non-reinforced, Standard GradeInformation provided by Toyobo.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0060 - 0.012 cm/cm

@Thickness 1.60 mm
0.0060 - 0.012 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax CCP PBT 3040-201 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0060 - 0.012 cm/cm

@Thickness 1.60 mm
0.0060 - 0.012 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax CCP PBT 5615-104C 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..