Physical Properties Metric English Comments
Linear Mold Shrinkage 0.013 - 0.017 cm/cm

@Thickness 3.17 mm
0.013 - 0.017 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-60/VO/NH Polypropylene Homopolymer, Flame Retardant, non-halogenated, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.013 - 0.017 cm/cm

@Thickness 3.17 mm
0.013 - 0.017 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0
Information provided by FIBERFIL Engineered Plastics