Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
Normal; ISO 294-4 |
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm @Thickness 2.00 mm |
0.019 in/in @Thickness 0.0787 in |
Normal; ISO 294-4 |
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic.. |