Polymer Property : Linear Mold Shrinkage = 0.024 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.020 - 0.024 cm/cm

@Thickness 6.35 mm
0.020 - 0.024 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.020 - 0.024 cm/cm

@Thickness 6.35 mm
0.020 - 0.024 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-61/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.020 - 0.024 cm/cm

@Thickness 6.35 mm
0.020 - 0.024 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-61/VO Polypropylene Copolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.020 - 0.024 cm/cm

@Thickness 6.35 mm
0.020 - 0.024 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics