Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.030 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.030 cm/cm

@Thickness 12.7 mm
0.030 in/in

@Thickness 0.500 in
ASTM D955
Fiberfil® PP-60/TC/13 BL8860 Polypropylene Homopolymer, 13% Talc Filled
Information provided by FIBERFIL Engineered Plastics