Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 0.46 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.46 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow UNIVAL™ DMDA-6320 NT 7 High Density Polyethylene Resin (HDPE) Low swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6320 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package household.. |