Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 0.85 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.85 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow FLEXOMER™ GRSN-1539 NT 7 Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ GRSN-1539 NT 7 is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins .. |
|||
Melt Index of Compound | 0.85 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.85 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow FLEXOMER™ DFDA-1010 NT 7 Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1010 NT 7 is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins .. |