Physical Properties Metric English Comments
Melt Index of Compound 110 g/10 min

@Load 21.6 kg,
Temperature 190 °C
110 g/10 min

@Load 47.6 lb,
Temperature 374 °F
cm<sup>3</sup>/10 min
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman