Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 230 °C |
18 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs SN0 ABS Information provided by Polykemi AB |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 230 °C |
18 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs V0X ABS, Flame Retardant Information provided by Polykemi AB |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 260 °C |
18 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 260 °C |
18 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 260 °C |
18 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Asia Pacific) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Melt Index of Compound | 18 g/10 min @Load 2.16 kg, Temperature 260 °C |
18 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Melt Index of Compound | 18 g/10 min @Load 2.16 kg, Temperature 260 °C |
18 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Asia Pacific) Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Melt Index of Compound | 18 g/10 min @Load 2.16 kg, Temperature 260 °C |
18 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 260 °C |
18 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® HCX1640 PC+ABS (Europe-Africa-Middle East) CYCOLOY™ HCX1640 a PC+ABS blend specially developed for medical devices and pharmaceutical applications requiring improved mechanical performance . It combines good flow with excellent impact and l.. |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 260 °C |
18 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 220 °C |
18 g/10 min @Load 11.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer Improved flow PC with excellent processability and mold release. |
|||
Melt Index of Compound | 18 g/10 min @Load 1.20 kg, Temperature 300 °C |
18 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 916R PC (Europe-Africa-Middle East) Lexan* 916R Polycarbonate (PC) resin is a low viscosity, non-filled, injection molding grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating at 0.8 mm properties. Lexan* .. |
|||
Melt Index of Compound | 18 g/10 min @Load 1.60 kg, Temperature 250 °C |
18 g/10 min @Load 3.53 lb, Temperature 482 °F |
cm³/10min; ISO 1133 |
PolyOne Bergadur™ PB40 G15 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Melt Index of Compound | 18 g/10 min @Load 1.20 kg, Temperature 300 °C |
18 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD4413 PC (Asia Pacific) Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Melt Index of Compound | 18 g/10 min @Load 1.20 kg, Temperature 300 °C |
18 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® LUX2110T_ PC (Europe-Africa-Middle East) Global grade. LEXAN LUX2110T is an injection moulding grade especially designed for manufacturing optical parts requiring easy flow properties combined with very high transmission and color stabilit.. |
|||
Melt Index of Compound | 18 g/10 min @Load 1.20 kg, Temperature 300 °C |
18 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® LUX2114G PC (Europe-Africa-Middle East) Lexan LUX2114G (EXRL0943) is a diffusive, mid viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develope.. |
|||
Melt Index of Compound | 18 g/10 min @Load 1.20 kg, Temperature 300 °C |
18 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® LUX2180T_ PC (Europe-Africa-Middle East) Global grade. LEXAN LUX2180T is an injection moulding grade especially designed for manufacturing optical parts requiring easy flow properties combined with very high transmission and color stabilit.. |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 260 °C |
18 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 260 °C |
18 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Asia Pacific) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Melt Index of Compound | 18 g/10 min @Load 2.16 kg, Temperature 250 °C |
18 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® FXV310SK PBT (Europe-Africa-Middle East) LIMITED USE, No New Customers / Applications as of Jan. 2010: VALOX FXV310SK is an unreinforced PBT injection moulding resin with high flow characteristics and containing a metal sparkle Visual FX. .. |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 260 °C |
18 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 250 °C |
18 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® XD1588 PBT+PC (Europe-Africa-Middle East) PBT+PC blend for painted automotive exterior applications, having good flow. |
|||
Melt Index of Compound | 18 g/10 min @Temperature 230 °C |
18 g/10 min @Temperature 446 °F |
ASTM D1238 |
Toyobo PELPRENE™ P80C Polyester TPE, High Flexibility, High Melting Point Features: Polyester TPE, High Flexibility, High Melting PointInformation provided by Toyobo. |
|||
Melt Index of Compound | 18 g/10 min | 18 g/10 min | Condition 190/21.6, HLMI; ASTM D1238 |
Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin Resin Type: Medium molecular weight distributionCharacteristics: Combination of toughness and tensileGood puncture resistanceMeets FDA regulations for food packaging below cooking temperaturesInform.. |
|||
Melt Index of Compound | 18 g/10 min @Load 2.16 kg, Temperature 230 °C |
18 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow C702-20NA Polypropylene Impact Copolymer Resin OverviewHigh impact performanceContains a nucleating additiveContains an antistatic additiveComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C702-20NA Polypropylene Resin is intended f.. |
|||
Melt Index of Compound | 18 g/10 min @Load 2.16 kg, Temperature 190 °C |
18 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Engage® 8411 Polyolefin Elastomer Description: Engage® 8411 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in durable injection molded industrial and consumer goods and compression molded gask.. |
|||
Melt Index of Compound | 18 g/10 min @Load 2.16 kg, Temperature 230 °C |
18 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
A.D. Compound Adene NC180A Homopolymer 15% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Melt Index of Compound | 18 g/10 min @Load 5.00 kg, Temperature 220 °C |
18 g/10 min @Load 11.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Asia Pacific) Improved flow PC with excellent processability and mold release. |
|||
Melt Index of Compound | 18 g/10 min @Load 2.16 kg, Temperature 300 °C |
18 g/10 min @Load 4.76 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PX2391 PPE+HIPS (Europe-Africa-Middle East) PX2391 is a 10% glass fiber reinforced, heat stabilized, low odor and low emission NORYL(R) grade for interior automotive applications, especially instrument panels |
|||
Melt Index of Compound | 18 g/10 min @Load 2.16 kg, Temperature 250 °C |
18 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |