Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 34 g/10 min @Load 2.16 kg, Temperature 265 °C |
34 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Melt Index of Compound | 34 g/10 min @Load 2.16 kg, Temperature 265 °C |
34 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Melt Index of Compound | 34 g/10 min @Load 2.16 kg, Temperature 265 °C |
34 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Melt Index of Compound | 34 g/10 min @Load 2.16 kg, Temperature 250 °C |
34 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Melt Index of Compound | 34 g/10 min @Load 2.16 kg, Temperature 250 °C |
34 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V2000DM PBT (Europe-Africa-Middle East) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Melt Index of Compound | 34 g/10 min @Load 2.16 kg, Temperature 250 °C |
34 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V2000DM PBT Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |