Polymer Property : Melt Index of Compound = 36 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 36 g/10 min

@Load 1.20 kg,
Temperature 300 °C
36 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer
Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.
Melt Index of Compound 36 g/10 min

@Load 1.20 kg,
Temperature 300 °C
36 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® HP1HF PC
Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable.
Melt Index of Compound 36 g/10 min

@Load 1.20 kg,
Temperature 300 °C
36 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® HP1HF PC (Europe-Africa-Middle East)
Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable.
Melt Index of Compound 36 g/10 min

@Load 1.20 kg,
Temperature 300 °C
36 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Asia Pacific)
Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.
Melt Index of Compound 36 g/10 min

@Load 1.20 kg,
Temperature 300 °C
36 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® HP1HF PC (Asia Pacific)
Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable.
Melt Index of Compound 36 g/10 min

@Load 21.6 kg,
Temperature 190 °C
36 g/10 min

@Load 47.6 lb,
Temperature 374 °F
MVR, [cm<sup>3</sup>/10 min]
Huntsman IROGRAN® A 85 P 5350 TPU-Polyester
Introduction: IROGRAN A 85 P 5350 is a flame-retardant, halogen-free, polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 5350 is par..
Melt Index of Compound 36 g/10 min

@Load 2.16 kg,
Temperature 260 °C
36 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
Mitsui APELâ„¢ APL5014DP Cyclo Olefin Copolymer (COC)
This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces..
Melt Index of Compound 36 g/10 min

@Temperature 230 °C
36 g/10 min

@Temperature 446 °F
ASTM D1238
Amco PRIMATOP PP CO 350-20 Impact Polypropylene Copolymer
PP CO 350-20 has easy mold flow and excellent dimensional stability. It is used in thin walled injection molded applications.Former A-Top Polymers product; part of Amco product line since 2013.