Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 40 - 48 g/10 min @Load 2.16 kg, Temperature 240 °C |
40 - 48 g/10 min @Load 4.76 lb, Temperature 464 °F |
ASTM D1238 |
Shinkong Synthetic Fibers Shinite® D201K002 PBT, Low Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Melt Index of Compound | 40 - 48 g/10 min @Load 2.16 kg, Temperature 240 °C |
40 - 48 g/10 min @Load 4.76 lb, Temperature 464 °F |
ASTM D1238 |
Shinkong Synthetic Fibers Shinite® D201K002 PBT, Low Viscosity Information from Shinkong Synthetic Fibers Corp. |
|||
Melt Index of Compound | 38 - 48 g/10 min @Load 2.16 kg, Temperature 190 °C |
38 - 48 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group EVATANE® 33-45 Copolymer Ethylene - Vinyl Acetate EVATANE® 33-45 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-45 is stabilized with antioxidants. The High Vinyl Acetate co.. |