Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 55 g/10 min @Load 21.6 kg, Temperature 190 °C |
55 g/10 min @Load 47.6 lb, Temperature 374 °F |
cm<sup>3</sup>/10 min |
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS.. |
|||
Melt Index of Compound | 55 g/10 min @Load 21.6 kg, Temperature 190 °C |
55 g/10 min @Load 47.6 lb, Temperature 374 °F |
cm<sup>3</sup>/10 min |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melt Index of Compound | 55 g/10 min @Load 21.6 kg, Temperature 190 °C |
55 g/10 min @Load 47.6 lb, Temperature 374 °F |
cm<sup>3</sup>/10 min |
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo.. |
|||
Melt Index of Compound | 55 g/10 min @Load 21.6 kg, Temperature 190 °C |
55 g/10 min @Load 47.6 lb, Temperature 374 °F |
MVR, [cm<sup>3</sup>/10 min] |
Huntsman IROGRAN® A 91 P 4945 TPU-Polyester Introduction: IROGRAN A 91 P 4945 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 91 P 4945 is part of the HUNTSMAN technical ext.. |
|||
Melt Index of Compound | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8350 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Melt Index of Compound | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow 959S Linear Low Density Polyethylene (LDPE) DOW Polyethylene 959S is a medium molecular weight distribution homopolymer. This resin has good process-ability over a wide range of molding conditions. Typical applications include lids. It com.. |
|||
Melt Index of Compound | 55 - 80 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 - 80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group EVATANE® 42-60 Copolymer Ethylene - Vinyl Acetate EVATANE 42-60 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE 42-60 is stabilized with antioxidants and contains slip and antibloc.. |