Polymer Property : Melt Index of Compound = 66 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 66 g/10 min

@Load 2.16 kg,
Temperature 190 °C
66 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow DMDA-8965 NT 7 High Density Polyethylene Resin
DOW DMDA-8965 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as food containers. Information provided by Dow