Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 70 g/10 min @Load 5.00 kg, Temperature 280 °C |
70 g/10 min @Load 11.0 lb, Temperature 536 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Rynite® RE19051 BK507 PET
(Unverified Data**) Rynite® RE19051 BK507 is a 40% glass and mineral reinforced, flame retardant, polyethylene terephthalate black resin.Information provided by DuPont Performance Polymers |
|||
Melt Index of Compound | 70 g/10 min @Load 21.6 kg, Temperature 210 °C |
70 g/10 min @Load 47.6 lb, Temperature 410 °F |
cm<sup>3</sup>/10 min |
Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 95 R 4813 is a thermoplastic polyester- polyurethane for injection moulding applications. Additional characteristics of the product are very short cycle times and high dimens.. |
|||
Melt Index of Compound | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5020 400 Micron LDPE Powder Description: ICOFLO 510-5020 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5056 500 Micron LDPE Powder Description: ICOFLO 510-5056 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5057 80 Micron LDPE Powder Description: ICOFLO 510-5057 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5058 1200 Micron LDPE Powder Description: ICOFLO 510-5058 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOTEXâ„¢ 520-5019 300 Micron LDPE Powder Description: ICOTEX 520-5019 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and a .. |
|||
Melt Index of Compound | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOTEXâ„¢ 520-5056 500 Micron LDPE Powder Description: ICOTEX 520-5056 is a low density polyethylene powder that has been developed to meet the special requirement of the textile coating industry. Key Characteristics: very high flow, very g.. |
|||
Melt Index of Compound | 70 g/10 min @Load 10.0 kg, Temperature 345 °C |
70 g/10 min @Load 22.0 lb, Temperature 653 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM SF2260 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
Melt Index of Compound | 70 g/10 min @Load 2.16 kg, Temperature 250 °C |
70 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® HX215HP PBT High Flow, Unreinforced, Polybutylene Terephthalate (PBT). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food conta.. |
|||
Melt Index of Compound | 70 g/10 min @Load 5.00 kg, Temperature 275 °C |
70 g/10 min @Load 11.0 lb, Temperature 527 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP THERMOCOMP RX07034 PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RX07034 is a compound based on PA 66 resin containing Glass Fiber. Added features include; Low Smoke, Easy Molding, Cross Linkable under Beta-or Gamma Radiation; Specially developed.. |
|||
Melt Index of Compound | 70 - 120 g/10 min | 70 - 120 g/10 min | |
Zig Sheng Industrial ZISAMIDE® HP3402 Nylon 6 ZISAMIDE® HP3402 is a spinning grade Polyamide 6. Application: textile brightInformation provided by ZIG SHEN Industrial Co., LTD. |
|||
Melt Index of Compound | 70 - 125 g/10 min | 70 - 125 g/10 min | |
Zig Sheng Industrial ZISAMIDE® TP4407 Nylon 6 ZISAMIDE® TP4407 is a Polyamide 6. Application: compounding extrusionInformation provided by ZIG SHEN Industrial Co., LTD. |
|||
Melt Index of Compound | 70 g/10 min @Load 2.16 kg, Temperature 190 °C |
70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group BONDINE® HX 8290 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride BONDINE® HX 8290 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. This grade is characterised by a high fluidity. Due.. |