Physical Properties Metric English Comments
Viscosity 0.0100 - 8.00 cP
0.0100 - 8.00 cP
Average value: 4.10 cP Grade Count:4
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu..