Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.503 cP | 0.503 cP | |
LG Chemical Methyl Acrylate Features: Low Color - Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Through the multistag.. |